Water-based thick plate pulp operation process, many customers can not achieve the expected results when printing, immediately think that there is a problem with the quality of thick plate pulp, in fact, the real reason is also very much related to the operation process, the following through the professional The technical staff introduced, let's look at how to operate when using water-based thick plates.

Waterborne ink method / step
1,80-150 mesh yarn (imported Japanese yarn), using a 45 degree (angle) mesh to pull the net, the angle of the font is clearer.
2, can also choose different meshes according to the requirements of the pattern, (Note: the screen must be tight, this is quite critical)
3, in order to ensure the printing effect, generally according to different needs to print thick version of white glue 4-7 times, each time generally 3-5 times, depending on the situation, the fastness requirements of the high thick transparent paste plus 1-3% of the additives are first made.
4, thick plate printing finished products need to pass through the drying tunnel (120 ° C -160 ° C) for 5-7 minutes, so as not to affect the fastness. It can also be naturally dried, and the natural drying time is related to temperature and air humidity.